環氧地坪施工前的設計和專業化施工隊伍的組織對基層的檢查和處理正確的施工組織和質量監督等過程的全程控制。在無錫環氧地坪漆施工前,須清楚了解查看基面狀況,下面介紹一般環氧地坪工業環氧地坪漆涂料涂裝對地面基層的要求及常見的處理方法。1)水泥基面牢固、結實、不起殼,應杜絕砂漿起殼現象,混凝土層與砂漿找平層最好一起澆筑。若先澆筑混凝土層,則要求砂漿層的厚度不低于40MM,對叉車道的要求則更厚。有關坡度應符合設計要求,允許偏差值的2%,并且不大于30MM。
(2)要求表面不起砂,硬度高,沒有水泥粉化現象。新澆筑的水泥砂漿要充分保養。水泥基面平坦,無凹凸不平、蜂窩麻面、水泥疙瘩、其他涂料、乳膠漆、泡泡糖等殘渣。(3)表面干燥,含水率小于6%,無油污,PH值應在6.0~8.0;水泥地面養護期過后進場施工前5D,基層不能再用水沖洗或被濕潤。
(2) No sand on the surface, high hardness and no cement powdering are required. The newly poured cement mortar should be fully maintained. The cement base surface is flat, without rugged, honeycomb linen, cement bumps, other coatings, latex paint, foam sugar and other residues. (3) The surface is dry, the moisture content is less than 6%, no oil pollution, and the PH value should be 6.0-8.0. After the maintenance period of cement ground, the base can no longer be washed or wetted with water 5 D before construction.
2、基層的檢查與預處理基層是環氧樹脂地坪涂料的基礎,要進行詳細檢查與分析,以確定其處理措施。
2. The inspection and pretreatment of the base is the basis of epoxy floor coatings. Detailed inspection and analysis are needed to determine the treatment measures.
(1)測量抗壓強度。工業環氧地坪的抗壓強度不應低于24MPa,為滿足某些承重要求,還可能需要更高的強度,應使用回彈儀進行強度測量,或取芯塊實測抗壓強度。
(1) Measure the compressive strength. The compressive strength of industrial floors should not be less than 24 MPa. In order to meet some important requirements, higher strength may be needed. Strength measurement should be carried out by rebound meter or coring.
(2)確定黏結強度?;炷粱鶎颖砻鎺缀撩缀穸葍韧ǔJ撬酀{形成的低強度層。因水泥水化反應導致的收縮,溫度變化或荷載的反復作用等產生的應力,會導致黏結強度降低。黏結強度不應低于1.5MPa。
(2) Determine the bond strength. The low strength layer formed by cement slurry is usually in the thickness of several millimeters on the surface of concrete base. The stress caused by shrinkage, temperature change or repeated action of load caused by hydration reaction of cement will lead to the decrease of bond strength. The bond strength should not be less than 1.5 MPa.
(3)基層含水率。只有在水泥基層含水率不大于6%的情況下才能進行涂料的施工,所以含水率的測量尤為重要。確定基層含水率的最佳方法是塑料薄膜覆蓋實驗法,即將至少1mX1m的聚乙烯薄膜用膠帶封粘在混凝土面上,待至少24小時后,根據塑料薄膜上出現冷凝水的數量確定含水率。
(3) Water content of grass-roots. Only when the moisture content of cement base is not more than 6%, can the coating be applied, so the measurement of moisture content is particularly important. The best method to determine the moisture content of the base course is the plastic film covering experiment method, that is, at least 1mX1m polyethylene film is sealed on the concrete surface with tape, and after at least 24 hours, the moisture content is determined according to the amount of condensation water appearing on the plastic film.
(4)環境溫度。忽略施工環境溫度因素可導致環氧地坪的質量缺陷,例如黏結強度降低、水印、空洞、不規則表面及硬化不兗分等。因此,對于環境溫度(氣溫)、基層表面的溫度、露點溫度等數所數據,在施工中必須每天測量數次。
(4) Environmental temperature. Ignoring the temperature factors of construction environment can lead to quality defects of epoxy floor, such as reduced bond strength, watermarking, voids, irregular surface and hardening. Therefore, the environmental temperature (air temperature), the surface temperature of the grass-roots, dew point temperature and other data, in the construction must be measured several times a day.
(5)基層清理。對于油脂、機油或有機酸、無機酸或水泥漿所引起的污染,如果不進行徹底清除,將影響環氧地坪漆涂料層的黏結性能。因此地,必須用機械方法清理表面,并通過測定黏結強度進行檢查。
(5) grass-roots clean-up. For oil, oil or organic acid, inorganic acid or cement slurry pollution, if not thoroughly removed, will affect the bonding performance of epoxy floor paint coating. Therefore, the surface must be cleaned mechanically and checked by measuring the bond strength.
3、基層處理
3. Grass-roots treatment
(1)為使無錫環氧地坪涂料的施工達到良好的效果,對于尚未找平的地面,應首先施工水泥找平層以進行找平處理。土建方找平時,在水泥初凝時,用專業地面機械對地面進行磨平處理。經過基層處理再涂裝的環氧涂裝地坪的表面會更平整、光亮,使用壽命也會提高。
(1) In order to achieve good results in the construction of epoxy floor coating, cement leveling layer should be first applied to leveling the ground that has not yet been leveled. When the cement is initially solidified, the civil engineer uses professional ground machinery to grind the ground. The surface of epoxy-coated floor will be smoother, brighter and the service life will be improved after basic treatment and re-coating.
(2)待水泥層干燥后(大約28天),用打磨機對地面進行整體打磨處理,使其表面平整,水泥毛細孔全部敞開。
(2) After the cement layer is dried (about 28 days), the whole ground is polished with a grinder to make the surface smooth and the cement capillary holes open.
(3)對于有油污(食用油、機油)的基層,先用表面處理劑噴灑于用水沖濕的地表面,反復擦洗,直到無油污為止。
(3) For the base layer with oil contamination (edible oil, engine oil), the surface treatment agent is sprayed on the surface wetted with water and scrubbed repeatedly until there is no oil contamination.
保證環氧地坪施工質量的五個關鍵技術要點鹽城環氧地坪 環氧地坪漆施工工藝說難很難、說簡單也很簡單,只要掌握好五個要點,就能保證地坪漆的施工質量,做出讓客戶滿意的鹽城環氧地坪施工工程。下面就給大家介紹環氧地坪漆施工過程中的五個要點:環氧地坪漆質量問題,80%以上都是施工技術上出現問題,因此,在進行環氧地坪漆施工時一定要嚴格把好關,每一道涂層都要注重… 環氧地坪漆?對基層地面處理的重要性鹽城環氧地坪 如果對環氧地坪漆的光澤度要求不高,可以在無錫環氧地坪漆完工后在表面罩一層啞光漆,這樣在光線下就不會特別明顯,而且還能有效提高環氧地坪漆的硬度。環氧地坪漆通常由環氧樹脂,溶劑和固化劑及顏料,助劑構成,其主要特征是與水泥基層的黏結力強,能夠耐水性及其他腐蝕性介質的作用以及具有非常良好的涂膜物理力…推薦新聞
如何處理環氧地坪施工后的起皮和起皮問題?…
一、環氧地坪漆產品質量因素底漆附著力差,環氧樹脂材料質量差,會造成地板耐久性、剝離、分層、變色、開裂等,應使…
在鹽城環氧地坪施工注意事項及其改造修補方…
在我們的生活中,鹽城環氧地坪漆是較為常見的一類涂漆了,不管是在各個企業的車間內,還是各個教育機構的教室內,我…
解析環氧地坪施工中涂附著力差的原因
環氧地坪中涂的作用是增加地坪的厚度,提高地坪的耐磨性能,作為找平層提高地坪的平整性;如果地坪中涂層附著力差,…
在鹽城施工高質量的環氧地坪我們需要注意哪…
質量好的鹽城環氧地坪一般可以使用5~8年時間,而質量不好的則會在半年之內出現弊病甚至損壞。發生這樣問題40%的原因…
建筑施工人員合理選擇環氧地坪五點須知
環氧地坪是現代建筑行業用的比較多的一種建筑材料。地坪裝飾行業最突出的特點是涂料和涂裝的整體結合,涂裝和涂層體…
環氧地坪多少一平方?鹽城環氧地坪施工報價…
環氧樹脂地坪系列包括環氧平面涂層,環氧砂漿地坪,環氧自流平地坪,環氧彩砂地坪,環氧防滑地坪,環氧防靜電地坪等…
環氧地坪地坪基層處理不好將會有哪些影響?…
熟話說,根基不穩,在強勢的產品終究還會下降的。環氧地坪也是如此,鹽城環氧地坪有地坪基層,相當于建房子的地基一…
環氧地坪包工多少錢?怎么施工才性價比高
環氧地坪哪家好?哪里便宜?提起這個問題,我相信大家都是公說公有理,婆說婆有理。要拿出真本事來,才算是好的。其…
水性環氧地坪與普通環氧地坪有何不同之處
水性環氧地坪最早在修建范疇得到了廣泛運用,今后才推行運用于鋼結構防腐涂料,水性環氧地坪是當前用于工業重防腐范…
在鹽城地下停車場使用環氧地坪的四大理由
現在很多商場小區都有地下停車場,我們都知道,地下停車場的環境比較潮濕,所以很多地下停車場都有使用環氧地坪,下…
管理員
該內容暫無評論